Fine ceramics (advanced ceramics, advanced technical ceramics) — Mechanical properties of ceramic composites at room temperature — Determination of compressive properties
Версия 2
2019-07
В время отменен
ISO 20504:2019
72346
Отозвано (Версия 2, 2019)

Тезис

This document describes procedures for determination of the compressive behaviour of ceramic matrix composite materials with continuous fibre reinforcement at room temperature. This method applies to all ceramic matrix composites with a continuous fibre reinforcement, uni-directional (1D), bi-directional (2D) and tri-directional (xD, with 2 < x < 3), tested along one principal axis of reinforcement or off axis conditions. This method also applies to carbon-fibre-reinforced carbon matrix composites (also known as carbon/carbon or C/C). Two cases of testing are distinguished: compression between platens and compression using grips.

Общая информация

  •  : Отозвано
     : 2019-07
    : Отмена международного стандарта [95.99]
  •  : 2
  • ISO/TC 206
    81.060.30 
  • RSS обновления

Жизненный цикл

Цели в области устойчивого развития

Данный стандарт разработан для достижения следующих Цель устойчивого развития

Появились вопросы?

Ознакомьтесь с FAQ